Gold-Tin Soldering

Gold-tin (AuSn) soldering refers to the use of gold-tin alloys—most commonly the eutectic Au80Sn20 (80 wt% Au / 20 wt% Sn)—as a hard solder for high-reliability joining in lasers, photonics, and optoelectronic packaging.


Technical Information:


The eutectic composition melts sharply at approximately 280 °C (solidus = liquidus). Typical key properties include:


  • Thermal conductivity: ~57 W/m·K


  • Electrical resistivity: ~16.4 μΩ·cm


  • Coefficient of thermal expansion (CTE): ~15.9–16 ppm/°C


  • Tensile strength: ~275 MPa


  • Young’s modulus: ~68 GPa


  • Density: ~14.5–14.7 g/cm³


It is a hard solder that forms stable intermetallic compounds (primarily Au₅Sn and AuSn) upon solidification. These provide high mechanical strength, excellent creep and corrosion resistance, and a moisture-impermeable barrier. Because of the high gold content, the alloy oxidizes minimally and supports fluxless soldering in vacuum, inert gas, or forming gas (N₂/H₂), which is critical for optics.


Common forms include stamped preforms, PVD/evaporated or electroplated thin films/bumps (typically a few to ~20 µm), and pastes. Reflow is usually performed at 300–320 °C. Surface tension during reflow can provide self-alignment (often to ~±1 µm), useful for optical coupling. Off-eutectic compositions (e.g., slightly Sn-rich) are sometimes used to accommodate gold metallization dissolution and still end at the desired eutectic joint.


Applications:


AuSn is the industry standard for many high-reliability photonic assemblies because of its combination of thermal performance, hermeticity, fluxless processing, and mechanical stability:


  • Laser diode die attach: Bonding high-power diode bars/stacks, DFB lasers, VCSELs, and GaN/InP lasers to heat sinks or submounts (Cu, AlN, Si, etc.). Efficient heat extraction improves efficiency, wavelength stability, and lifetime compared with softer solders such as indium.


  • Silicon photonics / PIC assembly: Flip-chip bonding of InP or GaAs laser sources to silicon photonic integrated circuits. Fluxless AuSn bumps avoid residue that would scatter light near waveguide facets; self-alignment helps achieve the tight tolerances needed for efficient coupling in high-speed (400G/800G/1.6T) transceivers and co-packaged optics.


  • Hermetic packaging: Lid sealing and feed-through attach in laser modules, optical transmitters/receivers, TOSA/ROSA packages, and other telecom-grade devices. The resulting joints support long-term reliability standards (e.g., Telcordia GR-468) by blocking moisture that degrades laser facets/mirrors.


  • Other: High-power LEDs, optical communication modules, LiDAR, and related RF/photonic hybrids where thermal management, high-temperature strength, and cleanliness are essential.


Compared with conventional soft solders, AuSn offers superior high-temperature strength, thermal conductivity, and reliability for power-dissipating photonic devices, at the cost of higher material price and greater brittleness. It is widely deposited as thin films or bumps for wafer-level and flip-chip processes in modern photonic packaging.